ABSTRACT

To restore oral functions in patients with missing teeth, single tooth implants are a well documented treatment option. The selection of the restorative materials should thus be based on the esthetic characteristics in addition to the biocompatibility and the strength characteristics. A focus of interest in implant dentistry; is the application of ceramic materials for the fabrication of the implant abutments as well as for prosthesis. Improved material characteristics, complying with clinicians’ and patients’ increased demands for highly esthetic results, have contributed significantly to the development of new generation of ceramic abutments. In the all-ceramic category, zirconia implant abutments provide a highly desirable option. The focus of this systematic review was to assess the published data concerning zirconia dental implant abutments from various aspects.

Key words: Zirconia, Implant, Abutments, Esthetics, Transformation toughening.

Dental implants are considered as an essential treatment modality which has demonstrated high success rates for replacement of both single and multiple teeth. However, this approach of rehabilitation is a clinical challenge especially in the anterior segment where esthetics has prime importance. One of the most challenging scenarios is to satisfy the patient expectations both functionally and esthetically. The high esthetic demands lead to the fabrication of metal free restorations using ceramic that exhibits ideal properties of biocompatibility and esthetics.1

The abutment is the portion of the implant that supports or retains a prosthesis or implant superstructure. The abutments are commonly made from materials, such as titanium, surgical stainless steel and gold. Of these, titanium has been the gold standard and continues its impeccable service with respect to biocompatibility and its physical property. In spite of the success of these materials there has never been a dearth in the efforts to formulate the right ceramic material to overcome the inherent esthetic compromise in the use of metals, especially with regard to anterior restorations.

The increased demand from patient for high esthetic result, and clinician’s need to achieve better treatment outcome, has considerably contributed to the development of a new generation of ceramic abutments. The materials of preference for ceramic abutments are densely sintered high purity alumina and yttria-stabilized tetragonial zirconia polycrystal ceramics. Alumina-based ceramics first broke into this ‘metal bastion’ and brought about the change that was so long desired and looked forward to. But as the first comer, its Achilles heel was that it possessed the risk of fracture during laboratory procedures and following abutment connection. To rein in this weakness, yttrium-oxide stabilized zirconia was introduced. It brought along several advantages like high flexural strength (900-1400 Mpa)2 and desirable optical properties. This material proved its worth in mechanical properties and reliability as a result of its stress-induced transformation toughening. Most modern abutments made from zirconia are now introduced in order to overcome the shortcomings and better complement the esthetics of a dental implant restoration.

In an in-vitro study by Yildrim3 et al the fracture resistance of such restorations were evaluated. Alumina and zirconia abutments were prepared and restored with glass-ceramic crowns and placed on Branemark implants (Nobel Biocare, Gathenburg, Sweden). No artificial aging was applied to the test specimens. The statistical analysis showed significant differences between both groups, with mean fracture load values of 280.1 N for the group with alumina abutments and 737.6 N for the group with zirconia abutments. The fracture resistance in the zirconia abutment was more than twice that in the alumina abutment group.

Ceramic abutments which were developed are available in prefabricated or customizable forms and can be prepared in the dental laboratory either by the technician or by utilizing computer aided design (CAD) manufacturing units.

ESTHETICS AND ZIRCONIA ABUTMENTS

Zirconia posesses maximal opaquing effect due to scattering of light by dispersed particles of zirconium oxide which are greater in size than wavelength of light and with a different refractive index to the matrix. Zirconia, though being a metal, has a very appreciable esthetic appeal due to its ‘tooth color’ and this factor alone takes it a long way in making it a very good choice as an implant abutment in the anterior region.

According to Watkin4, tissue discoloration in the cervical third of anterior implant restorations may result from implant abutment material show-through. As an alternative to metal abutments that may compromise the appearance of tissue color in the esthetic zone, zirconia abutments can be used. When zirconia abutments are combined with all-ceramic crowns, the appearance of the peri-implant tissue can be noticeably improved.

Also, the mechanical properties of zirconia are in a league of its own and poses a significant advantage over other esthetic abutment. This combination of more than acceptable esthetics and its far reaching mechanical properties make this the gold standard of esthetic material of all the ceramic materials available today.

Zirconia is a high strength ceramic, the yttria stabilized zirconia ceramic has twice the flexural strength of alumina ceramic (900-1400 MPa), a fracture toughness of upto 10 MPa/m0.5, and a modulus of elasticity value of 210 GPa. The enhanced strength of zirconia (ZrO2) can be explained by the microstructural differences, such as higher density, smaller particle size and polymorphic mechanism against flaw propagation.2,5

The main reason for the superior resistance of zirconia lies in the stabilizing effect of yttria, which allows the processing of zirconia in the metastable tetragonal crystalline structure at room temperature (18°C–23ºC). The tetragonal phase at room temperature allows for transformation to the monoclinic phase under stress and represents an efficient mechanism against flaw propagation. The transformation results in a compressive stress as the result of volume expansion and slows down further crack propagation, resulting in improvement of the mechanical properties (i.e. transformation toughening).1 It has been assumed that the phenomenon of transformation toughening contributes to this high fracture strength and the “self-repairing” properties of zirconium that prevent crack propagation.

It is the general understanding that ceramic abutments should demonstrate adequate resistance against the masticatory forces that rise during chewing or swallowing . To achieve a fine restoration, the abutment should present resistance to fracture to ensure long term success. In this aspect, zirconia abutments exhibit enhanced resistance. In addition, a cyclic fatigue pattern and stress corrosion fatigue caused by oral environment must be considered. In the oral environment, the inherent flaws of ceramic materials have been considered to induce propagation of crack to a critical size. A failure ultimately results from a final loading cycle that exceeds the mechanical capacity of the ceramics. A a rule of thumb, the endurance limit for fatigue cycling that can be applied to dental ceramics is approximately 50% of the maximum fracture strength. Consequently, it is reasonable to demand an initial fracture resistance within a safety range of 650 N for the anterior region and 1,000 N for the posterior region of maxilla and mandible, to ensure a favourable clinical prognosis of zirconium implant abutments and their all-ceramic restorations.

Further in vitro and in vivo studies are necessary to prove that this claim can be transferred to clinical situations. The zirconium-ceramic abutments investigated in a study conducted by Gehrke et al6 exhibited a maximum fracture strength of 672 N during a static loading and 269 N and 403 N during cyclic loading. This provides evidence that zirconium abutments can safely be used in the incisor region of the maxilla and mandible, while caution is recommended in the molar regions.

Yttria-stabilized tetragonal zirconia polycrystals (Y-TZP) implant abutments offer enhanced biocompatibility, metal-like radiopacity for better radiographic evaluation, and, ultimately reduced bacterial adhesion, plaque accumulation, and inflammation risk. Moreover, Y-TZP abutments may promote soft tissue integration, while peri-implant soft tissues may be clinically achieved adjacent to zirconia or alumina-zirconia abutments and zirconia healing caps.

Y-TZP abutments are available in two types: prefabricated and custom made. Prefabricated zirconia abutments are a reliable and practical solution but CAD/CAM technology is also beneficial in designing fully individualized zirconia abutments for ideal soft-tissue integration and esthetics. Both types of abutments give the opportunity for further customization either by extra-oral or intra-oral preparation.

The incidence of complications associated with zirconia abutments was determined by evaluating data from three studies.7,8,9 Glauser et al reported the clinical success of 36 experimental zirconia abutments on single-tooth implants, after a minimum observation period of 49.2 months. No abutment fractures were observed during clinical loading, resulting in a cumulative survival rate of 100%. Healthy peri-implant mucosa and stable marginal bone levels were documented at zirconia abutments.7 In another study, 30 zirconia abutments on single-tooth implants were observed after a follow-up period of 40 months. No abutments fractures or screw loosening were reported, resulting in a cumulative survival rate of 100%.8 Finally, a third study evaluated the success rate of 37 zirconia-alumina composite abutments (ZirAce, Acucera Inc., Reno, NV). Nine implants were single teeth, and 28 implants were FPDs. After a 12-month follow-up, no abutments fractures, cracks, screw loosening, or peri-implant infection signs were reported. In this study, neither zirconia-alumina abutment failures nor adverse soft tissue reactions were observed at 12 months.9 These studies indicate that zirconia abutments are suitable for clinical use.

Zirconia abutments may also represent a material surface less attractive for early plaque retention compared to titanium. Scarano et al reported a coverage by bacteria of 12.1% on zirconia as compared to 19.3% on titanium.10 Kou et al compared different polishing systems for zirconia and concluded that polishing creates surfaces similar to the just sintered ones and smoother than only grinding surfaces.11 These studies indicate that zirconium oxide can be suitable for implant abutment but more clinical and mechanical trials are necessary for a complete understanding of behaviour of zirconia abutments.

CONCLUSION

The diversity of contemporary materials and of methods available for the fabrication of implant supported, all-ceramic restorations makes it difficult to select the most appropriate treatment modality. New products are constantly being added to the wide range of existing products. For example, efforts are being made to produce low-temperature, degradation- free zirconia–alumina composites for dental implant abutments. The first short-term results are encouraging. Zirconia ceramics and abutments are being intensively investigated and are gaining in popularity. Future improvements in the ceramic will focus on its color and long-term stability. Attempts are being made to add coloring oxides to zirconia ceramic before the sintering process; this would change its whitish color and enhance the aesthetic outcome. It remains important, however, to verify the effectiveness of a suggested method before its recommendation.

Advances in computer-aided design⁄computer aided manufacturing technologies, which have made the fabrication procedures of ceramic abutments and implant-supported, all-ceramic restorations faster, easier, and more efficient, are playing a major role in the growing use of ceramic abutments. Future developments will make it possible to produce more resistant abutments and restorations with higher quality and lower fabrication time and costs.12

REFERENCES

  1. Varughese DP. Zirconia Abutments: A Quintessence of Modern Day Implantology. Int J Oral Implantol Clin Res 2012;3(3):133-7.
  2. Kohal RJ, Att W, Ba Chle M, Butz F. Ceramic abutments and ceramic oral implants: An update. Periodontology. 2008;47:224-43.
  3. Yildrim M, Fischer H, Marx R, Edelhoff D. In vivo fracture resistance of implant supported all ceramic restorations. J Prosthet Dent 2003;90:325-31.
  4. Watkin A, Kerstein RB. Improving darkened anterior peri-implant tissue color with zirconia custom implant abutments. Compend Contin Educ Dent 2008;29:238-40,42.
  5. Guazzato M, Quach L, Albakry M, Swain MV. Influence of surface and heat treatments on the flexural strength of YTZP dental ceramic. J Dent 2005;33:9-18.
  6. Gehrke P, Dhom G, Brunner J, Wolf D, Degidi M, Piattelli A. Zirconium implant abutments: fracture strength and influence of cyclic loading on retaining screw-loosening. Quintessence Int. 2006 Jan;37(1):19-26.
  7. Glauser R, Sailer I, Wohlwend A, et al: Experimental zirconia abutments for implant-supported restorations in esthetically demanding regions: 4-year results of a prospective clinical study. Int J Prosthodont 2004;17:285-90.
  8. Canullo L: Clinical outcome study of customized zirconia abutments for single-implant restorations. Int J Prosthodont 2007;20:489-93.
  9. Bae KH, Han JS, Seol YJ, et al: The biologic stability of alumina-zirconia implant abutments after 1 year of clinical service: a digital subtraction radiographic evaluation. Int J Periodontics Restorative Dent 2008;28:137-43.
  10. Scarano A, Piattelli M, Caputi S, Favero GA, Piattelli A. Bacterial adhesion on commercially pure titanium and zirconium oxide disks: An in vivo human study. J Periodontol 2004;75:292-6.
  11. Kou W, Molin M, Sjogren G. Surface roughness of five different dental ceramic core materials after grinding and polishing. J Oral Rehabil 2006;33:117-24.
  12. Jung YG, Peterson IM, Kim DK, Lawn BR. Lifetime-limiting strength degradation from contact fatigue in dental ceramics. J Dent Res 2000: 79: 722–31.

Disclaimer from Guident

The views and opinions expressed in articles published in Guident are solely those of the authors and do not necessarily reflect the views of the editors, the editorial board or the publisher, Ivory India. Guident does not endorse any product, technique or treatment described. Clinical content is intended for qualified dental and medical professionals and is not a substitute for individual clinical judgement. Guident, its editors and the publisher accept no liability for any consequence arising from the use of information published in the journal.

How to cite this article

Dr. Rajat Dang, Dr.Nikita Garg. Zirconia - the New Choic E for Implant Abutments. Guident. 2013 Nov;6(13). Available from: https://guident.net/articles/prosthodontics/zirconia-the-new-choic-e-for-implant-abutments.html

Related articles

More in Prosthodontics

All 444 articles
Vol. 7, Issue 1 · December 2013

Occlusal Reconstruction Using Composite Resin

Increasing numbers of people are presenting at dental offices with excessive occlusal wear and loss of vertical dimension that is both unsightly and physiologically dysfunctional…

Dr. Geoffrey M Knight

Call for papers

Publish your clinical work in Guident

Original research, case reports and review articles are welcomed from clinicians and researchers worldwide. Every submission is assessed by the editorial board.